Service Area: Worldwide
Company Location: United States
Raise the dumping test: Place it in the calibration environment for more than 12 hours, add 120 kg load, and continuously Plastic basin raise, dump, and drop more than 2000 times without cracks. In addition, static tests were carried out on empty and heavy-duty plastic drums on tilt surfaces with a tilt angle of 100. Plastic drums were not dumped.